There are so many materials for steel conveyor belts. Different material has these own characteristics:
More chemical analysis and material options, just browse the following chart:
Mark | Chemical Component | Oxidation Resistance Temperature (°C) |
Material Properties | ||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |||
45# Steel | 0.06–0.22 | 0.12–0.30 | 0.25–0.60 | – | – | – | – | – | – | 400 | |
D667 | 0.12 | 1.00 | 11.0–15.0 | 0.045 | 0.03 | 0.5–1.5 | 12.5–14.0 | 0.60 | 1.5–2.5 | Nickel steel grade, cold workability and corrosion resistance. | |
1Cr13 | 0.15 | 0.60 | 0.60 | – | – | – | – | – | – | 600 | |
1Cr18Ni9Ti | 0.12 | 0.60 | 0.60 | – | – | – | 12.0–14.0 | – | – | 750 | |
SUS304 (0Cr18Ni9) |
0.08 | 1.00 | 2.00 | 0.045 | 0.03 | 8.0–10.0 | 18.0–20.0 | – | – | 750 | Has good corrosion resistance and is widely used. |
New SUS304 (06Cr19Ni10) |
0.08 | 1.00 | 2.00 | 0.045 | 0.03 | 8.0–11.0 | 18.0–20.0 | – | – | 750 | Has good corrosion resistance and is widely used. |
SUS304H | 0.06–0.10 | 1.00 | 2.00 | 0.045 | 0.03 | 8.0–11.0 | 18.0–20.0 | – | – | Good corrosion resistance and high strength after cold working. | |
SUS304HC | 0.08 | 1.00 | 2.00 | 0.045 | 0.03 | 8.0–10.0 | 18.0–20.0 | – | 2.0–3.0 | 750 | Good cold workability, good corrosion resistance. |
SUS304M | 0.06 | 1.00 | 2.00 | 0.045 | 0.03 | 9.0–10.0 | 18.0–20.0 | – | – | 800 | Good corrosion resistance, good drawing performance. |
SUS316 | 0.08 | 1.00 | 2.00 | 0.045 | 0.03 | 10.0–14.0 | 16.0–18.0 | 2.0–3.0 | – | 800 | Corrosion resistance is superior to SUS304 in seawater and various organic acids. |
SUS316L | 0.03 | 1.00 | 2.00 | 0.045 | 0.03 | 12.0–15.0 | 16.0–18.0 | 2.0–3.0 | – | 800 | Has lower carbon content than SUS316 and better resistance to intergranular corrosion. An important corrosion resistant material. |
SUS310S | 0.08 | 1.50 | 2.00 | 0.045 | 0.03 | 19.0–22.0 | 24.0–26.0 | – | – | 1,000 | Heat resistance, good oxidation resistance. |
SUS314 | 0.25 | 1.5–3.0 | 2.00 | 0.040 | 0.03 | 19.0–22.0 | 24.0–26.0 | – | – | 1,000 | Good oxidation resistance, mostly used as heat resistant steel. |
Cr20Ni80 | 0.05 | rest | 0.05 | 0.020 | 0.02 | 75.0–78.0 | 19.0–21.0 | – | – | 1,350 | High temperature and carbon resistance. |
Cr25Ni35Si2 | 0.05 | ≤ 1.5 | 0.50 | 0.020 | 0.02 | 33.0–36.0 | 23.0–26.0 | rest | – | 1,250 | High temperature and carbon resistance. |
Cr25Ni20Si2 | 0.05 | ≤ 1.5 | 0.50 | 0.020 | 0.02 | 19.0–21.0 | 23.0–26.0 | rest | – | 1,250 | High temperature resistance. |
Alloy steel Containing Nb |
0.02 | ≤ 2.0 | 2.00 | 0.050 | 0.03 | 20.0–22.0 | 23.0–26.0 | 2.0–3.0 | – | 1,400 | High temperature resistance and hydrogen embrittlement. |
SUS201CU | 0.12 | 1.00 | 7.5–10.0 | 0.045 | 0.03 | 3.5–5.5 | 13.5–16.0 | 0.50 | 2.0–3.0 | Nickel steel grade, cold workability and corrosion resistance. | |
Note: In the above table, the listed components indicate the range, the rest is the maximum value. |
Inquiry for Our Product
Boegger Industech Limited
E-mail: sales@mesh-belts.com
When you contact us, please provide your detail requirements. That will help us give you a valid quotation.